gold loading 0.5 weight percent, titanium loading 0.5 weight percent; Na:Au atomic ratio, 1:1; obtained by impregnation of silica with sodium chloroaurate, titanyl acetylacetonate followed by calcination in air T=160°C; P=760.051 Torr; 24 h; Heating; Conversion of starting material;