反应条件
Cu; Mg; Ni in melt Sonication; mixt. of Al-Si, Mg, Ni, Cu, Fe melted (resistance furnace, 820-850 °C, complex modification by P (Cu-14percentP) and Ce, La (Al-Ce, La)), held at 740-780 °C, poured into preheated cup, ultrasound applied for 60 or 120 s; detd. by EDX;
参考文献
Journal of Alloys and Compounds, , vol. 492, # 1-2 p. 482 - 487