sodium methylate
T=25 - 30°C; 1.5 h; anodic oxidation: carbon-paste plate as anode, stainless-steel plate as cathode, constant current intensity of 1A, an anodic density of 63 mA/cm2; Further byproducts given;
sodium methylate
T=25 - 30°C; 1.5 h; anodic oxidation: carbon-paste plate as anode, stainless-steel plate as cathode, constant current intensity of 1A, an anodic density of 63 mA/cm2; Further byproducts given;
sodium methylate
T=25 - 30°C; 1.5 h; anodic oxidation: carbon-paste plate as anode, stainless-steel plate as cathode, constant current intensity of 1A, an anodic density of 63 mA/cm2; Further byproducts given;