hydrogen; cobalt(II) oxide; Al2O3 (sulphided); molybdenum(VI) oxide
T=300°C; P=112509 Torr; 4 h; further products: N-2-pentylpiperidine, N-3-pentylpiperidine, pentenes; also investigated: various metal oxide ratios in catalyst; various catalysts, also not sulphided; other time (1 h); Product distribution;
参考文献
Cerny, Mirko; Kraus, Milos
Collection of Czechoslovak Chemical Communications, 1981 , vol. 46, # 6 p. 1348 - 1354