1percent Pt, 0.4percent K, 2.4percent Sn, 5percent La and 91.2percent La-Ce-ZrO2 support; activated with H2 at 400 deg C T=525°C; P=2250.23 Torr; 1 h; tubular reactor; Product distribution / selectivity;
参考文献
BASF SE
Patent: US2009/326287 A1, 2009 ;
Location in patent: Page/Page column 14 ;